Features
High Velocity coatings produce not only harder, denser carbide coatings, but are also more ductile. Due to the lowered particle temperature there is less shrinkage and this combined with a simultaneous peening effect as the next particle arrives, produces lower residual stresses and enables a much greater thickness to be applied. These properties make the coatings significantly more wear resistant, especially where loads are high or erosion is prevalent. Normal Plasma type coatings usually fail due to the break up of the coating and not through wear of the particles. A resistant barrier layer provides the corrosion resistance of the alloy materials, hence the reason why coating density is so important. High Velocity Systems ensure there is no degradation.
HVOF coatings can apply materials that include Tungsten Carbide which makes coatings with exceptional wear protection – up to 10 times greater than hard-chrome plating for example. The process lends itself to high value applications, significantly extending the life of components such as mud rotors, gate and ball valves in the oil/gas sector or hard chrome replacement of aircraft landing gear or hydraulic pistons.
- Retention of powder chemistry due to the reduced time at temperature.
- There is lower oxide content due to there being less in-flight exposure time.
- There is higher density (lower porosity) due to there being greater particle impact velocities.
- Improved corrosion protection due to there being less through-thickness porosity.
Benefits of HVOF with Typical Coatings
- Tungsten Carbide – If this material is overheated, not only does it oxidise and lose carbide to carbon dioxide, but the carbide also becomes dissolved with in the Cobalt Matrix. The resultant mixed Tungsten/Cobalt Carbides are hard, but brittle. In some circumstances this is not very important, for example, when impact loads are low and wear is by stress abrasion. On the other hand, in applications such as tool and die parts and compressor blades subject to hammer wear, ductility as well as harness is required.
- MCrALY’s – are a family of high temperature oxidation resistant alloys which are used in gas turbines. They offer protection by readily forming an adherent oxide film on their surface, which delays further oxidation. However, this readiness to form oxides means that normally coatings will contain oxidised particles. Research has shown that these oxide layers around the particles act as a path for further oxidation and penetration of the oxidising medium to the substrate. The lower the oxide contents of the coating, the better. Oxidation rates follow a parabolic law. In other words, if the temperature is doubled the oxidation rate goes up by four times. Thus, if the particle temperature can be kept lower the oxide content is significantly reduced.
- Corrosion Resistant Alloys, e.g. Inconel 625 – These alloys provide corrosion protection by providing a resistant barrier layer. Therefore, coating density is very important and once again, oxide layers form paths along which the corrosion medium can migrate. Therefore, once again, a low temperature, high velocity process is appropriate.