Resistance to High Temperature Corrosion

The absence of oxide scales and the high density of Kermetico HVAF coatings results in their superior per­formance in high temperature corrosion environ­ments.

In oxidizing and sulphurizing environments HVAF coatings of alloy 625 and alloy 671 substantially outperformed their counterparts sprayed with electric arc or HVOF coatings.

Weight Gain of Alloy 671 Coatings Sprayed with an Electric Arc, HVOF, and HVAF, after Testing in N2-1%H2S-1%HCl Gas at 400°C for 1,440 Hours.

The beneficial factor was that HVAF metal coatings efficiently sintered and formed diffusion zones with a substrate at elevated temperatures, afterward per­forming as a “solid metal.”

Such sintering and inter-diffusion are restricted in other thermal spray coatings because oxide scales are efficient bar­riers to diffusion.

Weight Gain of HVAF Alloy 671 Coatings and Stock Materials after Testing in Air at 700°C for 1,000 Hours.

Pages: 1 2 3 4 5 6